Your current position: Home >> Coating defects caused by improper use of atomic ash

Coating defects caused by improper use of atomic ash


 Coating defects caused by improper use of atomic ash

 
In the automobile coating process, the top coat is the last process of Z. with the continuous development of the automobile industry, many manufacturers now use baking paint. If there is a problem after finishing, it is Z troublesome. The following atomic ash manufacturers will make a brief introduction according to the problems in production.
 
1. The top coat foams after baking.
 
Scrape off the bubbles after the bubbles of the top coat and see which layer the bubbles are on. If the bubbles appear in the primer layer, the atomic ash is well combined with the primer, and the substrate treatment may not be in place; After blowing off the bubbles, it is found that there is a layer of primer on the atomic ash and the substrate. Then it may be that the primer is too thick or the primer is not dry enough.
 
2. Pinholes and depressions appear after baking the finish paint.
 
First of all, consider whether the pinhole has its own quality. Secondly, if pinholes appear when the quality of atomic ash is qualified, it is generally because the atomic ash coating and grinding technology is poor and the sand holes are not handled well. In addition, during the coating and scraping process, if the coating and scraping tool is improperly selected, it will also cause pinholes.
 
3. "Prickle" after baking the finish coat.
 
First, the climate is too humid and the water absorption of the atomic ash is too large. The polished atomic ash adsorbs a considerable amount of water. The topcoat is sprayed before the water volatilizes. A small amount of water is sealed under the paint film. Once heated, the water volume expands sharply and breaks through the paint film to form a "prickly heat". Second, the water absorption of atomic ash is qualified. After being dried by hot air, spray the top coat, and there is "prickly heat" after baking. Then it is possible that after spraying the top coat, the solvent enters the drying room before it volatilizes fully. In this way, because the surface of the top coat is closed soon, the residual solvent has to break through the paint film to form "prickly heat". Of course, it may also be the quality problem of the topcoat, or the mismatch between the polarity of the solvent and the topcoat


Prev What are the types of atomic ash
NextSteps for scraping atomic ash

Copyright © 2020 Changxing Baodi Environmental Protection Technology Co., Ltd all reserved Web Admin --> >>

浙公網安備 33052202000243號?浙ICP備17019658號

主站蜘蛛池模板: 免费看男女做好爽好硬视频 | 天天爱夜夜操 | 欧美亚洲国产精品久久久 | 一级欧美日韩 | 精品国产日韩一区三区 | 日韩精品第三页 | 一区二区三区在线视频播放 | 全黄毛片 | 国产一级一级一级成人毛片 | 国产手机在线αⅴ片无码观看 | 亚洲精品社区 | 欧美人与禽zoz0性伦交 | 色综合91久久精品中文字幕 | 国产午夜电影在线观看 | 伊人激情网 | 国产一区二区三区日韩欧美 | 偷拍第一页 | 欧美日韩亚洲一区 | a级精品国产片在线观看 | 日韩免费在线观看视频 | 夜色毛片永久免费 | 激情综合亚洲欧美日韩 | 精品一区二区久久久久久久网精 | 国产日韩欧美一区二区三区视频 | 日本成人a | 欧美精| 欧美精品第一页 | 欧美日本一道本 | 欧美人与曾 | 曰韩在线| 中国一级全黄的免费观看 | 欧美日韩一区二区三区在线观看 | 国产第一页精品 | 一区二区三区在线视频播放 | 国产精品久久久 | 欧美日韩国产精品 | 亚洲四区 | 久久免费视频网站 | 亚洲欧美在线观看一区二区 | 欧美一区二区在线观看 | 精品久久亚洲一级α |